New
Material : Chromic Oxide Rod
Thickness of coating : 0.4mm for single side after grinding
Craft : Rod flame Spraying
Hardness of Coating : HV1300
Surface Porosity : <1%
Surface Bonding Strength : 7-8kg/mm²
Surface Roughness : 0.4
Suite for 0.02-0.05mm steel wire, copper wire and enameled-wire
The Guide pulley made of of aluminium with enameled equipment is easy deformation and the sprayed ceramic coating if failure because of its thin edge and light weight while being sprayed with ceramic rod gun by plasma sprayed facility. Therefore, our company has introduced the whole sets of detonation spraying equipment system.
Specialized for Enameling machine pulleys, the heating to the piece is less during the explosion process but can obtain better high density coating, stronger adhesion.